Zainal Abidin, Nor Ishida and Martin, Darren and Atrens, Andrej (2011) Corrosion of high purity Mg, AZ91, ZE41 and Mg2Zn0.2Mn in Hank's solution at room temperature. Corrosion Science, 53 (3). pp. 862-872. ISSN 0010-938X, DOI https://doi.org/10.1016/j.corsci.2010.10.008.
Full text not available from this repository.Abstract
This work compared the corrosion of typical Mg alloys (AZ91, ZE41 and Mg2Zn0.2Mn) and high purity (HP) Mg in Hank's solution at room temperature and in 3% NaCl saturated with Mg(OH)2. Corrosion was characterised by the evolved hydrogen and the surfaces after immersion. Corrosion in Hank's solution was weakly influenced by microstructure in contrast to corrosion in the 3% NaCl solution. This is attributed to the formation of a more protective surface film in Hank's solution, causing extra resistance between the α-Mg matrix and the second phase. The alloys with substantial Zn contents had a shorter incubation period in Hank's solution. © 2010 Elsevier Ltd.
Item Type: | Article |
---|---|
Funders: | UNSPECIFIED |
Uncontrolled Keywords: | A. Magnesium; B. SEM |
Subjects: | T Technology > TJ Mechanical engineering and machinery |
Divisions: | Faculty of Engineering |
Depositing User: | Mr. Faizal Hamzah |
Date Deposited: | 01 Aug 2011 06:49 |
Last Modified: | 15 Nov 2019 02:02 |
URI: | http://eprints.um.edu.my/id/eprint/1898 |
Actions (login required)
View Item |