Sandu, V and Aldica, G. and Grigoroscuta, M. A. and Burdusel, M. and Pasuk, I and Ching, Y. C. and Ionescu, A. M. and Badica, P. (2022) Effect of polysilane addition on spark plasma sintering and superconducting properties of MgB2 bulks. CERAMICS INTERNATIONAL, 48 (21). pp. 31914-31922. ISSN 1873-3956, DOI https://doi.org/10.1016/j.ceramint.2022.07.127.

Full text not available from this repository.
Official URL: https://doi.org/10.1016/j.ceramint.2022.07.127

Abstract

Polycrystalline MgB2 bulk samples were produced by ex-situ spark plasma sintering (SPS) using the oxygen-free preceramic polymer additive poly(dimethylsilane) as a source for carbon doping and as a sintering aid. Two major effects were identified. One is the significant enhancement of the densification kinetics during sintering for all tested compositions. The second one is the improvement of the high field critical current density for a certain level of the poly(dimethylsilane) addition.

Item Type: Article
Funders: Consiliul National al Cercetarii Stiintifice (CNCS) Unitatea Executiva pentru Finantarea Invatamantului Superior, a Cercetarii, Dezvoltarii si Inovarii (UEFISCDI) [5PTE/2020 BIOTEHKER], Ministerul Cercetarii, Inovarii si Digitalizarii [PN030101], Ministerul Cercetarii, Inovarii si Digitalizarii [21N/2019], IIRG at University of Malaya [IIRG007B-19IISS]
Uncontrolled Keywords: Sintering; Superconductivity; Magnetic properties
Subjects: Q Science > QC Physics
Divisions: Faculty of Engineering > Department of Mechanical Engineering
Depositing User: Ms Koh Ai Peng
Date Deposited: 24 Jul 2024 08:16
Last Modified: 24 Jul 2024 08:16
URI: http://eprints.um.edu.my/id/eprint/46252

Actions (login required)

View Item View Item